HDT and VST Tests on Plastics (ISO 75 and ISO 306)

Traditionally silicone oil has been the most popular medium for performing heat deflection temperature (HDT) and vicat softening temperature (VST) tests on polymers. The test principle and procedure are simple, and although silicone oil based test systems are very well established, they can be used safely only up to a maximum temperature of 280°C.

High temperature polymers like Polyether Ether ketone (PEEK) and Polyetherimide (PEI) have an increasing demand in the polymer industry due to their higher mechanical and thermal properties. An alternative medium is required to test these high temperature polymers because they have HDTs and VSTs higher than the temperature at which silicone oil can be used. We used a CEAST HV500, which utilizes an aluminum oxide fluidized bath, to perform a range of HDT and VST tests for both high and low temperature applications according to ISO 75-1 & 2 and ISO 306 Method B, respectively. We tested different grades of PEEK, Polystyrene (PS), Polycarbonate (PC), Polyamide (PA), Polyphenylene Sulphide (PPS-40 % glass fillers), Polypropylene (PP-15 % glass fillers) at temperature ramps of 50ºC/h and 120ºC/h in compliance with the aforementioned ISO standards.

We compared the results obtained from the aluminum oxide system with those obtained from the traditional silicone oil systems for materials with HDT values less than 280°C. With a sample size of 12 specimens per batch, statistical analysis on HDT tests showed a very repeatable and reproducible result with a maximum difference of 5% between the two mediums. We recommend the aluminum oxide fluidized bath system to be used for high temperature polymers which have HDTs or VSTs higher than 280°C. Lower temperature polymers can also be tested with the aluminum oxide fluidized bath system as testing has shown good agreement with results obtained from traditional silicone oil systems.


About This Solution

Related Standards: ISO 75-1 | ISO 75-2 | ISO 306
Specimen Type: Rectangular
Materials: Plastics
Type of Test: Thermal
Business Sector: Consumer/Industrial Products
You are viewing a static image in place of an informative flash animation. Please download Adobe® Flash Player and refresh this page to view the animation.
Interested in this Solution?
Contact Us

Related Literature:

CEAST HDT Vicat Series Thermo-Mechanical Systems   CEAST HDT Vicat Series Thermo-Mechanical Systems

Our Labs

Instron application labs are used for both research and development, as well as testing customer samples to assist in finding the right equipment.
Contact our Application Specialists to determine the solution that's best for you!